① Use the international chemical element symbol and the national symbol to indicate the chemical composition, and use the Arabic Alphabet to indicate the component content:
For example: China, Russia 12CrNi3A
② Use fixed digit numbers to represent steel series or numbers; Such as: United States, Japan, 300 systems, 400 systems, 200 systems;
③ Use the latinka abyceda a poradie na formulár the sériové číslo, only to indicate the účel.
① Use element symboly;
② Čínština pinyin, otvorená krba oceľ: P; Varenie oceľ: F; Killed oceľ: B; Trieda A oceľ: A; T8: Špeciálne 8; GCr15: Guľa ložisko.
◆ Väzba oceľ, pružina oceľ, such as: 20CrMnTi 60SiMn, (s a málo častí per 10,000} to indicate C content).
◆ Nehrdzavejúca oceľ, zliatina nástroj oceľ (s a málo tisíciny z C obsah), such as: 1Cr18Ni91/000C (that is, 0.1%C), stainless C Less than or equal to 0.{}}.{{}8% such as 0Cr18Ni9, ultra-low carbon C Less than or equal to {{14}.03% such as 0Cr17Ni13Mo.
The American Iron Iron And Steel Institute uses three digits to label rôzny štandardný grades of kujný nerez oceľ. Among them:
① Austenitic stainless steels are marked with 200 and 300 series numbers, for example, some of the more common austenitic stainless steels are marked with 201, 304, 316 and 310.
② Ferit a martenzita nerez oceľ are zastúpené by 400 séria čísla. feritické nerezové oceľové je označené 430 a 446, martenzitické nerezové oceľové je označené 410, 420 a 440C, dvojfázové (austenitovo-feritové).
③ Nehrdzavejúca oceľ, zrážkovo kalená nehrdzavejúca oceľ a vysoká zliatiny s an železo obsah menej ako 50% are zvyčajne názov by patent názvy alebo ochranné známky.