Characteristics, Applications, Grades And Advantages Of Monel400 And K-500 Alloys

Characteristics, applications, grades and advantages of Monel400 and K-500 alloys

 

Monel is the trade name for a group of nickel alloys consisting primarily of nickel and copper, with trace amounts of iron, manganese, carbon and silicon. Monel is stronger than pure nickel and is known for its corrosion resistance to a variety of corrosive environments. The material was first developed in 1901 by Robert Crooks Stanley. The name "Monel" is a trademark of "Specialty Metals Corporation". Known as a superalloy, Monel has a face-centered cubic lattice structure in its microstructure. Monel 400 is approved as a structural material by the ASME Boiler and Pressure Vessel Code.

Monel alloy is a single-phase solid solution binary alloy with excellent mechanical properties at subzero temperatures. Monel alloy 400 has a specific gravity of 8.80, a melting temperature range of 1300–1350 degree , and a Poisson's ratio of 0.32. The table below provides the mechanical properties of Monel 400 material at room temperature.

Characteristics, applications, grades and advantages of Monel400 and K-500 alloys

Characteristics, applications, grades and advantages of Monel400 and K-500 alloys

Hot Working: Typical hot working temperature range for Monel is 648-1176 degree (1200-2150 degree F). Before starting thermal processing, the appropriate temperature must be determined

There are five types of Monel alloys commercially traded under ISO standards 6208 (plate, sheet and strip), ISO 9725 (forgings), ISO 9723 (rods), ISO 9724 (wire) and DIN 17751 (tubes and tubes). These Monel grades are:

Monel 400 or Alloy 400

Monel 401

Monel 404

Monel 405

Monel K-500

Monel 400: Monel 400 complies with the following standards: BS 3075, 3076 NA 13, DTD 204B and ASTM B164. Also known as Alloy 400, it has high strength, excellent corrosion resistance, good ductility and thermal conductivity. Typical applications for Monel 400 include heat exchangers, valves, marine engineering, chemical and hydrocarbon processing.

Monel 401: Monel 401 is widely used in professional electrical and electronic applications. The alloy has good weldability and good brazing properties via the gas tungsten arc process. Resistance welding is a very satisfactory method of joining materials. Monel 401 is covered by standard UNS N04401.

Monel 404: The composition of Monel 404 has been carefully tailored to provide a very low Curie temperature, low permeability and good brazing characteristics. Monel 404 can be used with common welding and forging techniques, but cannot be hot-worked. To obtain a better finish, cold working can be performed. Monel 404 is widely used in transistor packaging and ceramic-to-metal seals, complying with UNS N04404 and ASTM F96 standards

Monel 405: Mainly used for stocking of automatic screw machines, Monel 405 is designated as UNS N04405 and covered by ASME SB-164, ASTM B-164, Federal QQ-N-281, SAE AMS 4674 & 7234, Military MIL-N- 894, BS3072NA18, BS3073NA18, QQ-N-286, DIN 17750, ISO 6208, BS3075NA18, BS3076NA18, ASTM B 865, DIN 17752, DIN 17753, DIN 17754, QQ-N-286, SAE AMS 4676, A Code Case ISO 9723 , ISO 9724, ISO 9725, BS3074NA18, DIN 17751 and NACE MR-01-75. It is a free machining grade of alloy 400. The sulfur content is increased to 0.025-0.060%, resulting in nickel-copper sulfide, which improves machinability.

Monel K-500: The addition of aluminum and titanium to a nickel-copper base gives Monel K500 greater strength and hardness as well as excellent corrosion resistance. However, Alloy K-500 has a greater tendency to stress corrosion cracking in certain environments under age-hardened conditions. Monel K500 is particularly suitable for centrifugal pump shafts in marine service. Typical applications for K-500 alloy are instruments, oil well tools, electronic components, marine propellers, pump shafts, rotating impellers, scrapers, scrapers and oil well drill collars.

 