Jan 22, 2024 Zanechajte správu

316LSS Or Hastelloy, Which Material Is Resistant To High Temperature And Pressure?

316LSS or Hastelloy, which material is resistant to high temperature and pressure?

 

Hastelloy B-3
Hastelloy B-3 Product Overview
Hastelloy B-3 is a nickel-based high-temperature alloy composed of nickel, molybdenum, cobalt and other elements, with a nickel content of approximately 65%. Hastelloy B-3 nickel-based alloy material is an improved material based on Hastelloy B-2. It improves the thermal stability of the material, thereby improving the corrosion resistance. At the same time, it improves the hot forming and cold forming properties. In recent years, it has been increasingly used in the production and manufacturing of chemical equipment.
Mechanical properties of Hastelloy B-3 alloy sheet in solid solution state:

316LSS or Hastelloy, which material is resistant to high temperature and pressure?

316LSS or Hastelloy, which material is resistant to high temperature and pressure?

Hastelloy B-3 Features

1. Hastelloy B3 material has a high elongation, creating favorable conditions for cold forming.

Hastelloy B3 material is harder than austenitic stainless steel and has a greater tendency to work harden, so it requires greater pressure when cold forming or step forming.

2. When the cold forming deformation rate of Hastelloy B3 material is less than 10%, it will not affect the corrosion resistance of the workpiece, but during the welding process, the presence of residual stress may cause hot cracks in the weld. Therefore, for workpieces that need to be welded later, the influence of residual stress should be eliminated as much as possible.

3. Cold forming with severe deformation will increase the yield ratio of Hastelloy B3 material and increase the susceptibility to stress corrosion and cracking. Intermediate and final heat treatment processes are often used.

4. Hastelloy B3 material is very sensitive to oxidizing media and sulfur, phosphorus, lead and other low melting point metals at high temperatures.

 

Zaslať požiadavku

whatsapp

Telefón

E-mailom

Vyšetrovanie