Nickel Alloy 600 Seamless Pipe

Learn about Nickel Alloy 600 Seamless Pipe
Nickel Alloy 600 Tubing (also known as Inconel 600 Tubing) is a nickel-chromium alloy known for its excellent corrosion and oxidation resistance, especially at high temperatures. It is a versatile alloy used in a variety of applications, including chemical processing, aerospace, and nuclear power generation.
What are the standard Inconel 600 pipes?
These pipes conform to ASTM B167, B829, and B517 specifications. Pipes are available in various sizes according to ASTM, ASME, and API standards. Inconel 600 seamless pipes are available in diameters from 4 mm to 219 mm, while welded and EFW pipes are available in diameters from 5 mm to 1219.2 mm, with wall thicknesses ranging from 0.5 mm to 20 mm.

Inconel 600 Tubing Mechanical & Physical Properties
| Inconel Alloy 600 | |
| 8.47 g/cm3 | |
| 1413 ℃ (2580 ℃F) | |
| Psi – 95,000 , MPa – 655 | |
| Yield Strength (0.2%Offset) | Psi – 45,000 , MPa – 310 |
| 40 % |
Schedule table of Alloy 600 Pipe
|
3 1/2" IPS( 4.000"O. D.) |
1/8" IPS(.405"O. D.) |
|---|---|
|
SCH 40, 10, 160, 80, XXH |
SCH 40, 80 |
|
4" IPS(4.500"O. D.) |
1/4" IPS(.540"O. D.) |
|
SCH 40, 10, 160, 80, XXH |
SCH 40, 10, 80 |
|
5" IPS( 5.563"O. D.) |
3/8" IPS(.675"O. D.) |
|
SCH 40, 10, 160, 80, XXH |
SCH 40, 10, 80 |
|
6" IPS(6.625"O. D.) |
1/2" IPS(.840"O. D.) |
|
SCH 10, 5, 80, 40, 160, 120 XXH |
SCH 5, 40, 10, 160, 80, XXH |
|
8 " IPS(8.625"O. D.) |
3/4" IPS(1.050"O. D.) |
|
SCH 10, 5, 80, 40, 160, 120 XXH |
SCH 40, 10, 160, 80, XXH |
|
10" IPS(10.750"O. D.) |
1" IPS:(1.315′O. D.) |
|
SCH 10, 20, TRUE 80(.500), 40, 80 (.500), |
SCH 5, 40, 10, 160, 80, XXH |
|
12" IPS(12.750"O. D.) |
1-1/4" IPS(1.660"O. D.) |
|
SCH 10, 20, TRUE40(.406), 40(.375), SCH80(.500) |
SCH 40, 10, 160, 80, XXH |
|
14" IPS(14.000"O. D.) |
1-1/2" IPS(1.900"O. D.) |
|
SCH10(.188), SCH40(.375) |
SCH 40, 10, 160, 80, XXH |
|
16" IPS(16.000"O. D.) |
2" IPS(2.375"O. D.) |
|
SCH10(.188), SCH40(.375) |
SCH 40, 10, 160, 80, XXH |
|
18" IPS (18.000"O. D.) |
2 1/2" IPS(2.875"O. D.) |
|
SCH-40 (.375) |
SCH 40, 10, 160, 80, XXH |
|
3" IPS( 3.500"O. D.) |
|
|
SCH 5, 40, 10, 160, 80, XXH |
Chemical Compatibility chart of Uns N06600 Pipe and Tube
| 14.00 - 17.00% | ||
| 72.000% | ||
| C | 0.005 - 1.050% | |
| 6.00 - 10.00% | ||
| 0.05% Maximum | ||
| 1.00% Maximum | ||
| 0.03% Maximum | ||
| S | 0.0015% Maximum | |
| 0.05% Maximum | ||
| B | 0.0006% Maximum | |
| 0.03% Maximum | ||
| P | 0.0015% Maximum |

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.